Appearance
Surcharge
The overall action caused by the surcharge was considered destabilising in line with the single source principal; therefore, an unfavourable partial load factor was applied to both horizontal and shear surcharge actions even though the shear action is stabilising. The horizontal action was added to Ed and the shear was added to Rd in line with their stabilities. The opposite is true for stacked loads except in bearing when they are treated as unfavourable.
Uniformly Distributed Load
The live uniformly distributed vertical surcharge pressure,
Patch Load
This action is applied directly behind the back of the first block. The methodology for patch loading was taken from the Piling Handbook, 9th edition (2016), revision 2022, clause 4.9.15:
Figure 7: Patch surcharge loading diagram. Piling Handbook, 9th edition (2016), revision 2022 Fig 4.2
Where
To allow for dissipation of the load at increased depth, the handbook suggest employing the Krey method which provides an envelope that
When assessing a block, all pressures acting on the block and on the blocks above were considered. Since the distribution of
Stacked Load
Stacked loads encompass all loads applied to the top surface of the cope. Vertical stacked loads are simply summed into a force per meter on the cope with their point of application as an average of all the loads. Horizontal loads are also summed into a force per meter but their lever arm is always the distance from cope level to the toe of the blocks.